Hi,
After reading a few posts about people skipping the addition of Oxy altogether, I had another go today...
I've tried using just the Creme Developer and I didn't see any of the 'blooming' I had when using the Oxy added. I did my first 'test-run' yesterday (and an A3000 mouse) and I ended up with some white spots on the buttons and an overall 'blotchy' or uneven removal of the yellowing...
Today I tried it (no Oxy this time) on an old VIC-1515 printer. I was using a 40vol (12%) Creme Developer and brushed it on with a small (about 1/2 inch across) artists brush, reapplying/rebrushing every 45-60 mins.
However I seem to have the same issue as yesterday, with uneven removal of the yellowing. The brush-marks of the initial application were still quite noticeable, even after 6 hours outside in the sun.
Do you have any other suggestions on what I could try for a more even finish?
Possibly diluting the Creme Developer with distilled water?
I've heard some people use a much weaker (3%) solution (plus Oxy) with good results.
I'd like to get it down pat before I risk the front-panel of my A3000! :-)
Cheers,
Mike.